High-Performance Bainitic Steels
H. K. D. H. Bhadeshia
Abstract
The choreography of atoms during the course of the bainite transformation has major consequences on the development of structure. In particular, the scale and extent of the structure is dependent directly on the fact that the atoms move in a disciplined fashion. This information can be exploited to develop unconventional alloys - for example, rail steels which do not rely on carbides for their properties, and the hardest ever bainite which can be manufactured in bulk form, without the need for rapid heat treatment or mechanical processing.
Materials Science Forum 500-501 (2005) 63-74.
Download PDF file of paper.
html web version.
Download slide presentation.
Download high-resolution figures (eps format, zip archive).
Conference photographs.
Related Papers
-
"Hard Bainite"
ISIJ International, Vol. 43 (2003) 1238-1243.
C. Garcia Mateo, F. G. Caballero and H.K.D.H. Bhadeshia
-
"Effect of Plastic Deformation on the Formation of Acicular Ferrite"
Materials Science and Engineering A, Vol. 360A, 2003, 249-257.
C. H. Lee, H. K. D. H. Bhadeshia and H.-C. Lee
-
"Acceleration of Low-Temperature Bainite"
ISIJ International, Vol. 43 (2003) 1821-1825..
C. Garcia Mateo, F. G. Caballero and H.K.D.H. Bhadeshia
-
"Three-Dimensional Atom Probe Analysis of Carbon Distribution in Low-Temperature Bainite"
Scripta Materialia, Vol. 50, 2004, 1277-1281.
M. Peet, S. S. Babu, M. K. Miller and H. K. D. H. Bhadeshia
-
"Developments in Martensitic and Bainitic Steels: Role of The Shape Deformation"
Materials Science and Engineering A, Vol. 378A, 2004, pp. 34-39.
H. K. D. H. Bhadeshia
-
"Nucleation Theory for High-Carbon Bainite"
Materials Science and Engineering A, Vol. 378A, 2004, pp. 289-292.
C. Garcia-Mateo and H. K. D. H. Bhadeshia
-
"Tempering of a Hard Mixture of Bainitic Ferrite and Austenite"
Materials Science and Technology, Vol. 20, 2004, 814-818.
C. Garcia-Mateo, M. Peet, F. G. Caballero and H. K. D. H. Bhadeshia
-
"Large Chunks of Very Strong Steel"
Millenium Steel, Vol. 5, 2004, 25-28.
Also published in Spanish; Metalurgia e Materiais, 61 (2005) 106-109. Translated by Professor Fernando Rizzo.
H. K. D. H. Bhadeshia
-
"Kinetics of the Bainite Transformation"
Proceedings of the Royal Society of London, Vol. A460, 2004, 1710-1722.
H. Matsuda and H. K. D. H. Bhadeshia
-
"Bainite formation influenced by large stress"
Materials Science and Technology, Vol. 20, 2004, 1499-1505.
K. Hase, C. Garcia-Mateo and H. K. D. H. Bhadeshia
-
"Effect of 30 Tesla Magnetic Field on Transformations in a Novel Bainitic Steel"
Scripta Materialia, Vol. 52, 2004, pp. 461-466.
R. A. Jaramillo, S. S. Babu, G. M. Ludtka, R. A. Kisner, J. B. Wilgen, G.
Mackiewicz-Ludtka, D. M. Nicholson, S. M. Kelly, M. Murugananth and H.
K. D. H. Bhadeshia
-
"Very Strong Bainite"
Current Opinion in Solid State and Materials Science, Vol. 8, 2005, pp. 251-257.
F. G. Caballero and H. K. D. H. Bhadeshia
 |
 |