Abstract

The martensite-start and bainite-start temperatures have been determined in reheated, high-strength weld deposits, with each result associated with 95% coincidence limits. This helped define isothermal transformation temperatures where bainite can be obtained without the risk of unintentional transformation to martensite. It has been demonstrated, therefore, that coalesced bainite, which is detrimental to mechanical properties, can be generated isothermally without the possibility of confusion with autotempered martensite.

Science and Technology of Welding and Joining 13 (2008) 593-597.

Audio podcastAudio podcast     Study guidestudy guide

Resources and documents

 coalesced bainite formed during isothermal holding

Pearlite in steels
Published 2025
Audio summaries
Steels 5th edition Published 2024
Bainite 3rd edition Free download
Crystallography 1st edition Free download Audio, video summaries
Bainite at play Published 2026 video
Theory of transformations in steels Free download
Functional Materials Free book Hard copy
Phase transitions
Free book,
source (CC-BY)
Isolation Free download
rail steels
Rails, 2024
Audio summary
Bainite in Steels, Chinese edition Translation, 2020
Innovations in everyday engineering materials
Published 2021