Residual Stress and its Mitigation
-
"Residual Stress Part 1 - Measurement Techniques"
Materials Science and Technology, Vol. 17, 2001, 355-365.
P. J. Withers and H. K. D. H. Bhadeshia
-
"Residual Stress Part 2 - Nature and Origins"
Materials Science and Technology, Vol. 17, 2001, 366-375.
P. J. Withers and H. K. D. H. Bhadeshia
- "Residual Stress: Material Factors"
Handbook of Residual Stress and Deformation of Steel, eds G. Totten,
M. Howes and T. Inoue, ASM International, Materials Park, Ohio, 2002, 3--10.
H. K. D. H. Bhadeshia
- Transformation Temperatures and Welding Residual Stressing in Ferritic Steels"
Proceedings of PVP2007, ASME Pressure Vessels and Piping Division Conference, paper PVP2007-26544, San Antonio, Texas, 2007, pp. 1-8
J. A. Francis, H. J. Stone, S. Kundu, R. B. Rogge, H. K. D. H. Bhadeshia, P. J. Withers and L. Karlsson
-
"Developments in Martensitic and Bainitic Steels: Role of The Shape Deformation"
Materials Science and Engineering A, Vol. 378A, 2004, pp. 34-39.
H. K. D. H. Bhadeshia
- "Welding Residual Stresses in Ferritic Power Plant Steels"
Materials Science and Technology, Vol. 23, 2007, 1009-1020
J. A. Francis, H. K. D. H. Bhadeshia and P. J. Withers
- "Transformation Plasticity in Steel Weld Metals"
Proceedings of the 10th International Aachen Welding Conference, 22--25 October 2007
H. K. D. H. Bhadeshia, J. A. Francis, H. J. Stone, S. Kundu, R. B. Rogge, P. J. Withers and L. Karlsson
- "Crystallographic Texture of Stress-Affected Bainite"
Proceedings of The Royal Society A, 463 (2007) 2309-2328.
S. Kundu, K. Hase and H. K. D. H. Bhadeshia
- "Characterising Phase Transformations and their Effects on Ferritic Weld Residual Stresses with X-rays and Neutrons"
Metallurgical and Materials Transactions A 39A (2008) 3070-3078.
H. Dai, J. A. Francis, H. J. Stone, H. K. D. H. Bhadeshia and P. J. Withers
- "Effects of Filler Metal Transformation Temperature on Residual Stresses in a High Strength Steel Weld"
Journal of Pressure Vessel Technology, Vol. 131, 2009, 041401.
J. A. Francis, H. J. Stone, S. Kundu, H. K. D. H. Bhadeshia, R. B. Rogge, P. J. Withers and L. Karlsson

 |
 |